MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Old Hickory 54-S Kentucky Ball Clay
Categories: Ceramic; Clay; Ball Clay

Material Notes: This ball clay is a multi- purpose clay that has excellent pressing, extrusion, and casting qualities. It has a moderately fine particle size distribution and the high plasticity and dry strength is due in part to unique mineralogy of the clay. The low total carbon content provides excellent oxidation characteristics to a variety of ceramic process formulas.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.50 µm48% of particles less than
 0.63 µmMedian particle diameter
 1.0 µm60% of particles less than
 <= 5.0 µm84% of particles less than
pH 5.8
Soluble Sulfates 400 ppm
Specific Surface Area 22.4 m²/g
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.630 ksiDry Modulus of Rupture for 50% clay/50% flint, cast bars
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.1 %Cone 04, Linear Fired Shrinkage
 6.0 %Cone 3, Linear Fired Shrinkage
 6.5 %Linear Drying Shrinkage
 7.2 %Cone 11, Linear Fired Shrinkage
 
Component Elements PropertiesOriginal ValueComments
Al2O3 28.44 %
CaO 0.16 %
Fe2O3 1.28 %
K2O 0.89 %
Loss on Ignition(%) 9.62 %
MgO 0.42 %
Na2O 0.090 %
SiO2 57.09 %
TiO2 1.93 %
 
Descriptive Properties
Absorption (%)12.1Cone 04, Fired
 4.4Cone 11, Fired
 9.6Cone 3, Fired
CEC/MBI (meg/100 ml)8.9
Crude ColorLight Grey
Filtration (ml)21
Pyrometric Cone Equivalent (PCE)31-32
Water of Plasticity (%)32
Wet Sieve Residue (%)0.92Wet Sieve Residue, +200 mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOHC902 / 161981

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.