MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
EMS-Griltech Grilon® BA 3100 White Nylon 66/Nylon 6 Bi-Component Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 66 (PA66); Nylon 66 Fiber

Material Notes: Description: GRILON BA 3100 is the new core / sheath bi-component fiber based on PA 66/PA 6 with a sheath melting range from 215 - 225 °C. The fine count bi-component fiber guarantees an even distribution of the adhesive in the fiber bond. It is preferably used for thermofusing of nonwovens and yarns.

Data provided by EMS-Griltech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Fiber Count 2.20 dtex
 
Thermal PropertiesOriginal ValueComments
Melting Point 215 - 225 °CSheath
 
Descriptive Properties
ColorRaw White
LusterSemidull
Staple Length43 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Griltech Grilon® TN 2200 White Nylon 6 Fiber
EMS-Griltech Grilon® M 369 White Nylon 6 Fiber (Small Count)
EMS-Griltech Grilon® M 371 White Nylon 6 Fiber (Small Count)
Evonik VESTAMID® HTplus M1036 PA6T/X, GF60
Overview of materials for Nylon 66 Fiber

PGRIL374 / 43226

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.