MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Yuyao Zhonga G-30V PBT, 30% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Reinforced flame retardant PBT offers good creep resistance, good impact, good dielectric strength, good fatigue resistance, heat resistance, good dimensional stability, good flow and processability, good flammability. Reinforced flame retardant PBT is used for electric coil skeleton, electric plug-in unit, luminaire parts, integrated circuit parts, automobile engine shells, automobile by-pass valve control, etc

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccASTM D792
Linear Mold Shrinkage 0.00050 - 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 188 MPaASTM D790
Flexural Modulus 8600 MPaASTM D790
Charpy Impact, Notched 10.5 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 215 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 - 265 °CInjection Temp
Mold Temperature 60.0 - 100 °C
Drying Temperature 115 - 120 °C
Dry Time 6.00 - 8.00 hour
Injection Pressure 60.0 - 90.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PYUYZ052 / 281845

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.