MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Delrin® 100 AF Acetal Extruded Teflon® Filled Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: Delrin® AF 100 Acetal, 100 AF, Extruded Teflon Filled Acetal
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/cc
@Temperature 22.8 °C
ASTM D792
Water Absorption 0.20 %Immersion; 24hrs; ASTM D570(2)
Water Absorption at Saturation 1.0 %ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110(M80); ASTM D785
Hardness, Shore D 80ASTM D2240
Tensile Strength 6200 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 10 %ASTM D638
Tensile Modulus 360000 psi
@Temperature 22.8 °C
Elasticity; ASTM D638
Flexural Strength 12000 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 445000 psi
@Temperature 22.8 °C
Elasticity; ASTM D790
Compressive Strength 13000 psi
@Strain 10 %,
Temperature 22.8 °C
10% Deformation; ASTM D695
Compressive Modulus 250000 psiElasticity; 73°F; ASTM D695
Shear Strength 7.60 ksi
@Temperature 22.8 °C
ASTM D732
Izod Impact, Notched 0.600 ft-lb/inType "A"; ASTM D256
Coefficient of Friction, Dynamic 0.15
@Temperature 22.8 °C
(Dry vs Steel); PTM 55007
K (wear) Factor 40.0 x 10-10 in³-min/ft-lb-hrPTM 55010
Limiting Pressure Velocity 9000 psi-ft/minPTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.1ASTM D150
Dielectric Strength 400 kV/inShort Term; ASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F(TMA); ASTM E831
Melting Point 347 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 180 °F
Deflection Temperature at 1.8 MPa (264 psi) 244 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 1 L natural (4685) PA6 + PP, Dry, 30% Glass Filled
Delrin Delrin® 100 BK602 POM
Delrin Delrin® 100 NC010 POM
Delrin Delrin® 100AF POM-PTFE20
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)

P1SMDEL / 185310

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.