Pyrotek's I-28 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-28 also contains no RCF's. Applications - Thermal insulation
- Pot bake out panels
- Backup insulation
Advantages - Exceptional strength
- Asbestos-free
- Easily cut to specifications
- Composed of incombustible, inorganic material
- Can withstand temperatures up to 1093°C
Information provided by Pyrotek. |