MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ecomass® 4703ZC57 Stainless Steel Filled Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Nontoxic alternative to Lead (Pb), weighting and balancing applications
  • Moderate Specific Gravity
  • Stainless Steel Filled Polyurethane (TPU)
  • Flexible

Information provided by Technical Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.30 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3330 psiASTM D638
Elongation at Break 800 %ASTM D638
Tensile Modulus 80000 psiASTM D638
Flexural Strength 5800 psiASTM D790
Flexural Modulus 12600 psiASTM D790
Izod Impact, Notched 5.30 ft-lb/inASTM D256
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 430 °F
Mold Temperature 50.0 - 80.0 °F
Drying Temperature 200 °Fthen reduce to 160°F
Dry Time 2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elastomer Engineering E900-90A Polyurethane
Dow TONE™ 305 Polyol
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
Dow BETAMATE™ 7205 Polyurethane Prepolymer
Dow BETAMATE™ 7201 Polyurethane Prepolymer

PECOM58 / 35468

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.