MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Compound H Rust Proof
Categories: Fluid; Lubricant

Material Notes: Texaco Rust Proof Compounds deliver value through:
  • Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the elements. Good water displacing capabilities ensures that the protective film is also waterproof. The special rust inhibitor system ensures maximum protection against corrosive attack. Good penetrating characteristics ensure difficult-to-reach seams and crevices receive effective corrosion protection.
  • Minimum surface preparation required — Ability to penetrate existing flaky or heavy rust means that little or no preliminary cleaning of metal surfaces is required before application. This penetrating ability makes existing rust easier to remove, should it be considered desirable to do so for a better or more economical job.
  • Minimal cost — Self-sealing properties of the protective film minimizes the need for touch-ups when film damage occurs through scratches or brush marks. The overall cost of this soft film rust protection is much less than ordinary paint.
  • Easy removal — Soft protective film is readily soluble in petroleum solvent or kerosine to enable easy removal when required.

Texaco Rust Proof Compounds are soft film rust preventives designed for relatively long-term protection of iron and steel.

They are formulated from high melting point petrolatums and a special rust inhibitor system with penetrating and water displacing capabilities.

Texaco Rust Proof Compounds are recommended for:

  • Iron and steel exposed to atmospheric conditions before, during and after manufacturing into finished parts
  • Undercoating of vehicles
  • Transformer casings
  • Bridges and floating bridge pontoons
  • Nonfood storage vessels
  • Nonpotable water tanks
  • Ballast tanks
  • Gas holders
  • Hoisting equipment
  • Farm implements

May be applied by brush, dip or spray.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221977; MSDS Number: 9038

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 14225°C (77°F), Undisturbed
 
Thermal PropertiesOriginal ValueComments
Melting Point 69.0 °C
Minimum Service Temperature, Air 27.0 °CBrush
 54.0 - 66.0 °CSpray
 66.0 - 79.0 °CDip
Flash Point 243 °C
 
Descriptive Properties
Solvent, max, wt%0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA172 / 77051

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.