MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bakelite® PF 6680 Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Phenolic Molding compound, filled with glass fiber and glass beads, low abrasion, good chemical resistance

Applications: Thermally and mechanically highly stressed parts in automotive field, pistons, guidance elements, valve blocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/ccISO 1183
Apparent Bulk Density 0.780 g/ccISO 60
Linear Mold Shrinkage 0.0025 cm/cmInjection Molding. Post Shrinkage = 0.05%.; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 450 MPaH961/30; ISO 2039/P1
Tensile Strength 115 MPaISO 527 - 1/2
Tensile Modulus 20000 MPaISO 527 - 1/2
Flexural Strength 195 MPaISO 178
Flexural Modulus 14500 MPaISO 178
Compressive Strength 275 MPaISO 604
Charpy Impact Unnotched 14.5 kJ/m²ISO 179-1 eU
Charpy Impact, Notched 3.00 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 8.0 MPa 170 °CISO 75-2
 
Descriptive Properties
Water absorption (mg)1024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBAKE987 / 192349

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.