MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AE-9933 PPA, 33% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: Amodel® Supreme AE-9933 is a 33% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with outstanding dielectric strength at temperature. High thermomechanical performance provides excellent creep resistance. Low moisture absorption is also characteristic of this resin. The Amodel® AE family is specially formulated to work in the modern automotive and electrical & electronics markets, featuring non-corrosive stabilizers for increased performance at temperature. Very high mechanical performance at elevated temperatures, high heat deflection temperature, excellent hydrolytic stability, glycol resistance, and chemical resistance make this material an ideal candidate for metal replacement spanning automotive, aerospace, consumer, and industrial applications.

- Black: AE-9933 BK 324

Applications: Appliances; Automotive Applications; Automotive Electronics; Automotive Interior Parts; Automotive Under the Hood; Cell Phones; Connectors; Consumer Applications; Fuel Lines; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools

Features: Antifreeze Resistant; Chemical Resistant; Creep Resistant; Electrical Corrosion Resistant; Electrically Insulating; Good Dimensional Stability; Good Stiffness; Good Surface Finish; High Glycol Resistance; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Hydrolytically Stable; Low Moisture Absorption

Injection notes: Storage:
- Amodel® PPA compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® PPA resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® PPA processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccMethod A; ISO 1183
Water Absorption 0.16 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 199 MPaISO 527-2
 65.0 MPa
@Temperature 200 °C
ISO 527-2
 108 MPa
@Temperature 150 °C
ISO 527-2
 153 MPa
@Temperature 100 °C
ISO 527-2
Elongation at Break 2.1 %ASTM D638
 1.9 %
@Temperature 100 °C
ASTM D638
 2.7 %
@Temperature 150 °C
ASTM D638
 5.1 %
@Temperature 200 °C
ASTM D638
Tensile Modulus 12600 MPaISO 527-2
 800 MPa
@Temperature 100 °C
ISO 527-2
 4870 MPa
@Temperature 200 °C
ISO 527-2
 8880 MPa
@Temperature 150 °C
ISO 527-2
Flexural Strength 223 MPaASTM D790
 257 MPaASTM D790
Flexural Modulus 11200 MPaISO 178
Izod Impact, Notched 69.0 J/mASTM D256
Izod Impact, Unnotched 660 J/mASTM D256
Izod Impact, Notched (ISO) 8.40 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 37.0 kJ/m²ISO 180
Charpy Impact Unnotched 48.0 kJ/m²Type 1; ISO 179
Charpy Impact, Notched 7.40 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+16 ohm-cmASTM D257
Surface Resistance 2.40e+16 ohmASTM D257
Dielectric Constant 4.1
@Frequency 1e+6 Hz
ASTM D150
 4.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Dissipation Factor 0.017
@Frequency 1e+6 Hz
ASTM D150
 0.018
@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 600 VUL 746
 >= 600 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Temperature 150 - 200 °C
ISO 11359-2
 15.0 µm/m-°C
@Temperature 10.0 - 60.0 °C
ISO 11359-2
 16.0 µm/m-°C
@Temperature 60.0 - 110 °C
ISO 11359-2
 18.0 µm/m-°C
@Temperature -40.0 - 10.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C
@Temperature -40.0 - 10.0 °C
ISO 11359-2
 58.0 µm/m-°C
@Temperature 10.0 - 60.0 °C
ISO 11359-2
 65.0 µm/m-°C
@Temperature 60.0 - 110 °C
ISO 11359-2
Melting Point 327 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 319 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 304 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 318 - 332 °C
Middle Barrel Temperature 318 - 332 °C
Front Barrel Temperature 326 - 342 °C
Melt Temperature 332 - 354 °CInjection
Mold Temperature 180 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveLubricant; Mold Release
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4075 / 279875

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.