Properties: Chlorinated Polyethylene CPE-250 is a kind of CPE for plastic. Low chlorine content, high crystallinity and good compatibility with HDPE. Chlorinated Polyethylene CPE-250 can be used together with HDPE for production of cables with superior electrical performances.Information provided by Shanghai Potomer International Trade Co., Ltd |