MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese 50000430 n-Butyric anhydride
Categories: Fluid

Material Notes: CAS Number: 106-31-0

n-Butyric Anhydride is a clear, colorless liquid with an unpleasant, pungent odor. It is miscible in any proportion with most organic solvents. The product hydrates with water and decomposes with alcohol.

n-Butyric Anhydride may be used as an acylating agent, e.g. in the production of dyes, aromas and agrochemicals. It may also be used in the production of cellulose butyrate and cellulose aceto-butyrate.

Information provided by Celanese Corporation.

Key Words: n-Butanoic acid anhydride; (CH3CH2CH2CO)2O; (CH3CH2CH2CO)2O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.966 - 0.967 g/cc
Density 0.00659 g/ccVapor density
Viscosity 1.7 cP
@Temperature 20.0 °C
Molecular Weight 158.2 g/mol
Vapor Pressure 0.000400 bar
@Temperature 20.0 °C
Storage Temperature -17.8 - 37.8 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point -75.0 °C
Boiling Point 198 °C
Flash Point 88.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.413 - 1.415
@Temperature 20.0 °C
nD; DIN 51 423, part 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Cellulose Acetate Butyrate, Molded
Overview of materials for Polycarbonate, Molded
Overview of materials for Polypropylene, Molded
Overview of materials for Polysulfone (PSU)
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate

WCELAN920 / 177991

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.