MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description

Invision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weatherability.
Application

For extruded skin applications
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9015 sec delay; ASTM D2240
Tensile Strength, Ultimate 21.0 MPaat max load; ASTM D638
Elongation at Break 430 %ASTM D638
Flexural Modulus 0.190 GPaTangent; ASTM D790
Tear Strength 67.0 kN/mASTM D1938
 
Descriptive Properties
Colorfastness/Weatherability 2500 Delta E (kJ/m^2)SAE J1885

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® MT24F01 Medical Grade Acetal Copolymer
Celanese Celcon® MT8U01 Medical Grade Acetal Copolymer
Celanese Celcon® MT24U01 Medical Grade Acetal Copolymer
Celanese Celcon® MT12U03 Medical Grade Acetal Copolymer
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)

PASHU051 / 25015

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.