MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Constellium Certal® SPC Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in many types of applications. Typical applications include compression or injection moulds for plastics.

Information provided by manufacturer

Key Words: AA 7122 rolled
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.76 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 140
@Thickness 240 - 305 mm
 160
@Thickness 150 - 240 mm
Tensile Strength >= 490 MPa
@Thickness 240 - 305 mm
Tempers T651 / T652
 >= 510 MPa
@Thickness 150 - 240 mm
Tempers T651 / T652
 520 MPa
@Thickness 240 - 305 mm
Tempers T651 / T652
 530 MPa
@Thickness 150 - 240 mm
Tempers T651 / T652
Tensile Strength, Yield >= 430 MPa
@Strain 0.2 %,
Thickness 240 - 305 mm
Tempers T651 / T652
 >= 440 MPa
@Strain 0.2 %,
Thickness 150 - 240 mm
Tempers T651 / T652
 450 MPa
@Strain 0.2 %,
Thickness 240 - 305 mm
Typical Strength
 460 MPa
@Strain 0.2 %,
Thickness 150 - 240 mm
Typical Strength
Elongation at Break >= 2.0 %
@Thickness 240 - 305 mm
Tempers T651 / T652
 >= 4.0 %
@Thickness 150 - 240 mm
Tempers T651 / T652
 5.0 %
@Thickness 240 - 305 mm
Typical Elongation
 7.0 %
@Thickness 150 - 240 mm
Typical Elongation
Modulus of Elasticity 73.0 GPacompression
Tensile Modulus 72.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.873 J/g-°C
Thermal Conductivity 150 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.9 - 92.45 %as balance
Chromium, Cr <= 0.10 %
Copper, Cu 0.50 - 1.0 %
Iron, Fe <= 0.35 %
Magnesium, Mg 2.6 - 3.7 %
Manganese, Mn <= 0.10 %
Silicon, Si <= 0.25 %
Titanium, Ti <= 0.15 %
Zinc, Zn 4.3 - 5.2 %
Zirconium, Zr 0.15 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
Constellium Certal® SPC Forged Aluminum
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
304 Stainless Steel
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy

NCONS017 / 160280

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.