MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-FORM 5531 EMI Shielding Material
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed to be robotically dispensed using high pressure dispense equipment.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.20 g/ccASTM D792
Deformation 10 %4 N/cm
 20 %8 N/cm
 30 %15 N/cm
 40 %28 N/cm
 50 %52 N/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35ASTM D2240
Tensile Strength at Break >= 75.0 psiASTM D412
Compression Set 40 %ASTM D395 Method B 22 hrs 85°C
 40 %
@Temperature 85.0 °C,
Time 79200 sec
ASTM D395 Method B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0030 ohm-cmInitial; Chomerics MAT-1002
 0.0040 ohm-cmAged; Chomerics MAT-1002
Shielding Effectiveness 52 dB
@Frequency 1e+10 Hz
CHO-TP08
 55 dB
@Frequency 2.00e+9 Hz
CHO-TP08
 65 dB
@Frequency 6.00e+9 Hz
CHO-TP08
 67 dB
@Frequency 1e+9 Hz
CHO-TP08
 71 dB
@Frequency 2.00e+8 Hz
CHO-TP08
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 5.50 g/min
Cure Time 4.00 hour
@Temperature 22.0 °C
50% RH; Handling Time
 48.0 hour
@Temperature 22.0 °C
50% RH; Full Cure
Tack-Free Time 18.0 min
@Temperature 22.0 °C
50% RH
 
Descriptive Properties
Cure MechanismMoisture
FillerAg/Cu
ResinOne Part Silicone
Time for QC Measurements8 hrsElectrical Resistance and Adhesion @ 22°C 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive
NuSil R-2634 Silicone, Electrically Conductive
P & P Technology EC-S Pure Silver Loaded Silicone
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer

PCHOME087 / 28309

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.