MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress cracking. This product presents good processability for a wide range of mold conditions. This product complies with ASTM standard D1248-IA3.

Applications: Injection molding of toys and household utensils that need good Environmental Stress Cracking Resistance (ESCR). Production of Master Batch for dyeing and concentrate of additives such as slip agent, anti-block, anti-static, etc.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.

Information provided by Dax Resinas

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.916 - 0.920 g/ccASTM D1505
Viscosity 57 cP
@Shear Rate 3000 1/s,
Temperature 190 °C
ASTM D3835
 111 cP
@Shear Rate 1000 1/s,
Temperature 190 °C
ASTM D3835
 217000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
ASTM D3835
Melt Index of Compound 5.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8.50 MPaASTM D638
Tensile Strength, Yield 9.50 MPaASTM D638
Elongation at Break 300 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 230 µm/m-°C
@Temperature 20.0 °C
dilatation; ASTM D696
Thermal Conductivity 0.300 W/m-KASTM D177
Melting Point 110 °CASTM D3418
Vicat Softening Point 83.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 280 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Braskem PB 608 LDPE Injection Molding Polyethylene
Chevron Phillips KN 226B LDPE Injection Molding Resin
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade

PDAX079 / 29504

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.