MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Armacell AP Armaflex® SA 1 1/2" & 2" Self-Adhering Sheet & Roll Insulation
Categories: Other Engineering Material

Material Notes: The original, fiber-free, flexible elastomeric pipe, valve and duct insulation – with a laborsaving self-adhering system – for reliable protection against condensation, mold and energy loss. AP Armaflex FS SA is PVC free.
  • Self-adhering system makes application easy and reduces installation time
  • Fiber-free, formaldehyde-free, low VOC and non-particulating formulation protects indoor air quality
  • Closed-cell structure provides excellent condensation Control
  • Built-in vapor barrier eliminates need for additional vapor retarder
  • Microban® antimicrobial product protection inhibits the growth of mold and mildew in the insulation
  • 25/50 rated for use in air plenums: Up to 1" thickness in AP Armaflex 1-1/2" and 2" thickness in AP Armaflex FS
  • Thickness up to 2" with R-value up to R-8

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.20 %ASTM C209
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0360 W/m-K
@Temperature 24.0 °C
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
ASTM C177 or C518
Maximum Service Temperature, Air 82.0 °CASTM C534
Minimum Service Temperature, Air -183 °CASTM C534
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
R-ValueR-1.63/8"
 R-2.11/2"
 R-3.13/4"
 R-4.21"
 R-61 1/2"
 R-82"
Water Vapor Permeability0.05 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell AP Armaflex® White and Black Tube Insulation Through 1" Wall
Armacell AP Armaflex® SA Through 1" Self-Adhering Sheet & Roll Insulation
Armacell NH Armaflex® Nonhalogen insulation in flexible tubes, sheets and rolls
Armacell Armaflex® COIL Tube Insulation
Armacell Armaflex® 520 Adhesive

PARMD005 / 186616

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.