DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose applications. It is also recommended as a modifier in blends with flexible copolymers such as ethylene ethyl acetate (EVA) and ethylene ethyl acrylate (EAA) to enhance their rigidity in extrusion applications. Information provided by Dow |