Chemically inert, Dry Ground Bone Ash from Pyrotek is less dense than aluminum and will not effect the quality of castings. Bone Ash is a dry white coating which out performs red mud as a parting agent and adheres and packs well into troughs and launders. Its superior protection from skull build-up increases the life of trough sections, refractories and tools. Applications - Sealant for refractory cracks
- Dry coating for refractory parts and tools
- Glass manufacturing
- Parting agent
Advantages - Chemically inert
- Effectively releases skull
- Easy to apply
- Packs well into cracks
- Adheres to tools and refractories
Information provided by Pyrotek. |