MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorSafe™ HE3493-LS-H HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: BorSafe" HE3493-LS-H is a bimodal polyethylene compound produced by the advanced Borstar technology. The natural product is a readymade compound, including carefully selected stabilizers to ensure excellent long-term thermal stability and UV-resistance for limited outdoors storage of the final product. BorSafe HE3493-LS-H is classified as a PE100 material with MRS > 10 MPa. A PE100-RC material following the draft EN/ISO PE pressure pipe standards as currently revised. PE-RT Type II material where pipe pressure testing results between 20°C and 110°C are analyzed according to ISO 9080, showing conformity to the reference lines for PE-RT Type II rating. The grade is intended to be used for industrial applications.

Applications:

  • Industrial applications
  • Technical components exposed to high heat and loads
  • Cable protection pipes
  • Sheets and profiles
  • Relining
  • Glass fiber ducts
  • Co-extrusion of layers for pressure pipes
  • High temperature EHV- and HV- cable protection pipes
  • Geothermal applications and storage
  • Low temperature District Heating (4th generation)
  • Oil & Gas Applications
Specifications: EN ISO 15494; BorSafe HE3493-LS-H is intended to be used for industrial applications. Pipe testing has shown conformity to PE-RT Type II requirements of ISO 15494, ISO 24033, DIN 16833 and EN ISO 22391-2. The product meets the _PE100-RC_ Slow Crack Growth (SCG) requirements of EN 1555 and the draft standards under revision prEN 12201, ISO/DIS 4427 and ISO/DIS 4437.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccISO 1183-1
Oxidative Induction Time (OIT) >= 30.0 min
@Temperature 210 °C
ISO 11357-6
Melt Flow 0.230 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23.0 MPa50 mm/min; ISO 527-2
Elongation at Break >= 600 %50 mm/min; ISO 527-2
Tensile Modulus 950 MPa1 mm/min; ISO 527-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 210 °CCylinder
Die Temperature 200 - 210 °C
Melt Temperature 190 - 220 °C
Head Temperature 200 - 220 °C
Shelf Life 36.0 Month
 
Descriptive Properties
Accelerated Full Notch Creep Test>500 hin 2% Dehyton solution (4 MPa, 90 °C); ISO 16770
Accelerated Notched Pipe Test>300 hin 2% Arkopal N-100 solution (9,2 bar, 80 °C); ISO 13479
Cracked Round Bar>1.5 Million cyclesconverted to 14,0 mm and initial crack length 1,40 mm (12,5 MPa, 23°C); ISO 18489
Strain Hardening Modulus Test65 MPaISO 18488

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9662 / 323019

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.