EMERGE™ PC 6900 is a specially designed ignition-resistant polycarbonate alloy. It combines high flow, high heat and high strength together. It is especially suited for thin-wall applications and has excellent high gloss aesthetics. EMERGE™ PC 6900 has a UL 94 V-0 rating at 1.0 mm. This material does not contain chlorine or bromine additives. Main Characteristics: - Ignition resistant
- High flow
- High gloss
Applications:- Thin-Wall Powder Device Housings
- Consumer Electronics
- Information technology equipment