Description: SUPRALSIM® 690 is general steel plate for structure enables to make weight savings thanks to a minimum yield strength of 690 N/mm². Thanks to its exceptional purity rate (very low sulphur and phosphorous contents), and its adapted chemical analysis the SUPRALSIM® 690 steel is easy to shape and to weld. Information provided by manufacturer. |
EE 690 TIIK4 according to NFA 36-204, S690 QL according to EN 10137-2 |