MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik SANMAC 4571 Billet
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sanmac 4571, 1.4571/316Ti, is a titanium stabilized, molybdenum-alloyed austenitic chrome-nickel steel with improved machinability.

Information provided by Sandvik

ASTM 316Ti; UNS S31635; EN 1.4571

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 215
Tensile Strength, Ultimate 515 - 700 MPa
 >= 360 MPa
@Temperature 500 °C
 >= 375 MPa
@Temperature 300 °C
 >= 375 MPa
@Temperature 400 °C
 >= 390 MPa
@Temperature 200 °C
 >= 440 MPa
@Temperature 100 °C
Tensile Strength, Yield >= 210 MPa
@Strain 0.2 %
 >= 245 MPa
@Strain 1 %
 >= 129 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 135 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 145 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 158 MPa
@Strain 1 %,
Temperature 500 °C
 >= 164 MPa
@Strain 1 %,
Temperature 400 °C
 >= 165 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 175 MPa
@Strain 1 %,
Temperature 300 °C
 >= 185 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 192 MPa
@Strain 1 %,
Temperature 200 °C
 >= 215 MPa
@Strain 1 %,
Temperature 100 °C
Elongation at Break >= 40 %
Reduction of Area >= 50 %
Modulus of Elasticity 200 GPa
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
 17.5 µm/m-°C
@Temperature 30.0 - 300 °C
 18.0 µm/m-°C
@Temperature 30.0 - 500 °C
 18.0 µm/m-°C
@Temperature 30.0 - 400 °C
 18.5 µm/m-°C
@Temperature 30.0 - 600 °C
 19.0 µm/m-°C
@Temperature 30.0 - 700 °C
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.515 J/g-°C
@Temperature 200 °C
 0.525 J/g-°C
@Temperature 300 °C
 0.540 J/g-°C
@Temperature 400 °C
 0.555 J/g-°C
@Temperature 500 °C
 0.575 J/g-°C
@Temperature 600 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 200 °C
 18.0 W/m-K
@Temperature 300 °C
 20.0 W/m-K
@Temperature 400 °C
 21.0 W/m-K
@Temperature 500 °C
 23.0 W/m-K
@Temperature 600 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Chromium, Cr 17 %
Iron, Fe 67.4 %As Balance
Manganese, Mn 1.8 %
Molybdenum, Mo 2.1 %
Nickel, Ni 11 %
Phosphorus, P <= 0.045 %
Silicon, Si 0.40 %
Sulfur, S <= 0.030 %
Titanium, Ti >= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel

NSANDV185 / 19079

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.