MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TJPAPC PSM 145 High Heat for PS Foam
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Example Uses: Parts for large Home Electrical Appliances, Name Plates, Transparent Displays and Covers, Foamed PS

Information provided by Takht-e-Jamshid Pars Assaluyeh Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 1.8 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 480 kg(f)/cm²
Tensile Modulus 27000 kg(f)/cm²
Izod Impact, Notched 2.50 kg-cm/cm
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 99.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent, but not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
Tabriz WP 526 Performance Expandable Polystyrene
Entec Hyrene® PSCRY 14 General Purpose Polystyrene
Dow XIAMETER® PMCPMEM-0062 Emulsion PS
Dow Retain® PS-4378 Polystyrene

PTJPAPC988 / 197428

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.