MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Daplen™ EG107HP Polypropylene, 15% Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen™ EG107HP is a 15% mineral filled elastomer modified high performance polypropylene compound intended for injection molding. This material has a very good balance between impact strength and stiffness and gives an excellent surface quality.

Special Features:

  • Excellent scratch resistance
  • Available with and without UV-stabilization
  • Excellent surface appearance on unpainted parts
Applications:
  • Bumpers
  • Rocker panels
  • Body side moldings
  • Body panels
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.995 g/ccISO 1183
Melt Flow 22.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 20.0 MPa50 mm/min; ISO 527-2
Flexural Modulus 1750 MPa2 mm/min; ISO 178
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 100 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 - 80.0 °C
 230 - 280 °C
Mold Temperature 30.0 - 50.0 °C
Hold Pressure 30.0 - 60.0 MPa
 
Descriptive Properties
Flow front speed100 - 200 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9701 / 323058

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.