MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Universal Wire Works 347 Stainless Steel Electrode
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Universal 347 electrodes were developed for the welding of types 321 and 347 stainless and the clad side of steel clad with like alloys. Alloy 347 is used for the fabrication of equipment, which must be placed in service under severe corrosive conditions. Typical applications include pressure vessels for continuous service at temperatures of 700 to 1600 degrees F such as chemical plant and oil refinery equipment. Alloy 347 electrodes are columbium stabilized, containing columbium in the amount of 10 times the amount of carbon with a maximum of 1.00%. When welding stabilized alloys of 321 and 347, intergranular corrosion does not occur.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS E347-15,16
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 95000 psi
Elongation at Break 33 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.060 %
Chromium, Cr 19.4 %
Iron, Fe 67.2 %As Remainder
Manganese, Mn 1.9 %
Nickel, Ni 10.1 %
Niobium, Nb (Columbium, Cb) 0.80 %
Silicon, Si 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
347 Stainless Steel, cold drawn wire, 50% hard, 0.53-3.18 mm diameter
Overview of materials for T 300 Series Stainless Steel

NUWW026 / 19599

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.