MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Baytec® WE-180 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec WE-180 is a dicyclohexylmethane diisocyanate (HMDI)-terminated polyether prepolymer based on polytetramethylene ether glycol (PTMEG).

Properties / Applications: Baytec WE-180 is a dicyclohexylmethane diisocyanate (HMDI)-terminated polyether prepolymer based on polytetramethylene ether glycol (PTMEG). It is used in the formulation of two-component elastomer and binder systems. Polyurethanes from Baytec WE-180 prepolymer can be madeoptically clear, light-stable, and weather-resistant. They can range from rigid to flexible depending on the coreactant used. Typical uses include soft, energy-absorbing elastomers laminates for safety glasses, binders for dialysis filters and window gaskets. The material ’s low viscosity allows for easy production of complex parts with good surface definition. As with any product, use of the Baytec WE-180 prepolymer in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.055 g/cc
Viscosity 800 - 900 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength at Break 21.4 MPaASTM D412
Elongation at Break 100 %ASTM D412
Resilience 58Bayshore; ASTM D2632
Tear Strength 690 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 255 °CPMCC
 
Descriptive Properties
AppearanceColorless to pale yellow liquid
Content18.3-18.9%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8165 Urethane Casting
Elantas EN-2521 (Conap) Potting and Encapsulation Adhesive
Elantas EN-2527 (Conap) Potting and Encapsulation Adhesive
Elantas EN-2532 (Conap) Potting and Encapsulation Adhesive
Elantas EN-2541 (Conap) Potting and Encapsulation Adhesive

PCOVEST0269 / 202052

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.