MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Pocan® T 7323 POS151 000000 PBT+PET, 20% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 g/ccISO 60
Density 1.47 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %50% RH; ISO 62
Water Absorption at Saturation 0.40 %ISO 62
Viscosity Test 92 cm³/gViscosity Number; ISO 1628-5
Linear Mold Shrinkage, Flow 0.0040 cm/cm60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 175 MPaISO 2093-1
Tensile Strength at Break 120 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.2 %5 mm/min; ISO 527-1,-2
Tensile Modulus 7500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 195 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 195 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 7500 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -40.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 35.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Tensile Creep Modulus, 1 hour 7200 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 6100 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0018
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.260 W/m-KISO 8302
Melting Point 225 - 250 °C10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 150 °C20000 h (Electric strength); IEC 60216-1
 130 °C
@Thickness 1.50 mm
20000 h (Tensile impact strength); IEC 60216-1
 150 °C
@Thickness 1.50 mm
20000 h (Tensile strength); IEC 60216-1
Hot Ball Pressure Test 215 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °CISO 75-1,-2
Vicat Softening Point 210 °C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 0.800 mm
Oxygen Index 21 %Method A; ISO 4589-2
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, 60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °Cinjection molding; ISO 294
 260 - 280 °C
Mold Temperature 90.0 °Cinjection molding; ISO 294
 80.0 - 100 °C
Drying Temperature 120 °C
Dry Time 4.00 - 8.00 hour
Moisture Content 0.00 - 0.020 %Karl Fischer
 
Descriptive Properties
Specifications10.2°CHalving interval (Electric strength), IEC 60216-1
 10.2°CHalving interval (Tensile strength), 1.5 mm, IEC 60216-1
 13.5°CHalving interval (Tensile impact strength), 1.5 mm, IEC 60216-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 70G30HSL NC010 PA66-GF30
Celanese VECTRA MT1300 LCP, Medical Technology
Celanese Thermx® CG023 PCT, 20% Glass Reinforced
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned)
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)

PLANW9196 / 208467

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.