MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller KALAR® 5246 Elastomer
Categories: Polymer; Thermoplastic

Material Notes: KALAR® 5246 is a partially cross-linked butyl rubber compound pelletized for easy handling. KALAR® products feature all the performance attributes expected of butyl rubber. KALAR® 5246 is off-white in color and is the least cross-linked butyl rubber of the KALAR® series of products, providing an excellent butyl intermediate base for general-purpose sealants and tapes. Its controlled cross-linking facilitates easily compounded sealants that can be applied with a minimum of effort.

Features and Benefits: KALAR® 5246 has controlled cross-linking which makes it an ideal material for soft sealants with a greater degree of creep and slump resistance. Other key performance benefits include:

  • Elimination of butyl rubber pre-mastication
  • Pellets may be metered to facilitate mixing
  • Requires no vulcanization
  • Readily acceptable in a wide range of solvents
  • Extends with high levels of fillers and plasticizers
  • Compatible with a wide choice of compounding ingredients
  • Creep and cold-flow resistance
  • Compounding economy

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D71
Density 8.77 lb/galASTM D71
Mooney Viscosity 30 - 40
@Temperature 127 °C
ASTM D1646
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorOff-white
ConsistencyRubber Pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL242 / 317033

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.