MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Röhm PLEXIGLAS® Hi-Gloss 8N black 9V022 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: PLEXIGLAS® Hi-Gloss 8N black 9V022 is an amorphous thermoplastic molding compound (PMMA).

Typical properties of PLEXIGLAS® molding compounds are:

  • good flow
  • high mechanical strength, surface hardness and abrasion resistance
  • very good weather resistance
Special properties of PLEXIGLAS® Hi-Gloss 8N 9V022 are:
  • optimum mechanical properties
  • high heat deflection temperature
  • good flow / melt viscosity.
Application: PLEXIGLAS® Hi-Gloss 8N black 9V022 is particularly suitable for injection molding technical components. Owing to its superior brilliance, high-gloss (Class A) black surfaces can be obtained.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 1183
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 77.0 MPa5 mm/min; ISO 527
Elongation at Break 5.5 %5 mm/min; ISO 527
Tensile Modulus 3.30 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 20.0 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 103 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75
Vicat Softening Point 108 °CB / 50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 60.0 - 90.0 °CInjection Molding
Drying Temperature <= 98.0 °CPredrying
Dry Time 2.00 - 3.00 hourPredrying, Desiccant-Type Drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9372 / 319989

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.