MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Colmant Coated Fabrics EPDM Coated Aramid Tire Cord
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Tire cord fabric is a type of industrial fabric which is constructed using High Tenacity yarns in the warp direction and yarns of negligible resistance in weft direction which is used to hold warn yarns locked in their position. Tire cord coated fabrics provides fundamental properties such as controlled deformation, high strength, abrasion resistance, etc. Widely used by the tire industry, it is also employed for the rubber hose manufacture, air springs, expansion joints, among many other applications. Fiber consisting of a long chain polymer containing amines and aromatic components. Infusible, does not melt, does not burn, does not soften. Besides it shows low emission of toxic gases while combustion. Certain aramid can decompose at 500 ° C, It is thermostable up to 250 ° C. Ethlylene Propylene Diene Monomer is a copolymer of ethylene and propylene and a smaller amount of a diene monomer which forms chemically unsaturated ethylene groups pendant from the main saturated chain. These facilitate cross-linking reactions which do not affect the integrity of the polymer backbone. This feature gives EPDM excellent heat, ozone and chemical resistance. Physical properties are very good and resistance to polar fluids is generally good. Low temperature resistance is very good and EPDM can be compounded to give excellent electrical resistance.

Applications:

  • Expansion joints
  • Fireproof protection
Properties:
  • Non-skid
  • Oil storage
  • Ozone Resistance

Information provided by COLMANT COATED FABRICS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30 - 90
Tensile Strength at Break 8.00 - 20.0 MPa
Elongation at Break 100 - 900 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -55.0 °C
 
Descriptive Properties
IRHD Hardness30-90
Point Temperature-55 C° - 140C°
Warp breaking strength350 - 5000 daN/5cm
Warp elongation at break2% - 5%
Weft breaking strength350 - 2000 daN/5cm
Weft elongation at break2% - 5%
Weight per sqm100 - 650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLMANT017 / 316067

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.