MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Dow™ DNDA-1796 NT7 MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Product Description: Dow DNDA-1796 NT7 medium density polyethylene resin is produced via UNIPOL™ Process Technology. It also has utility in certain sheet applications and blow molding applications such as small, squeezable bottles. It exhibits high melt strength, excellent low temperature toughness, good stress cracking resistance, and outstanding flex life. It has a high molecular weight and a relatively broad molecular weight distribution that proves and excellent balance of performance properties and processability.
Main Characteristics:
  • High melt strength
  • Excellent low temperature toughness
  • Good environmental stress crack resistance
  • Excellent flex life
Complies with: ASTM D 3350: cell classification PE224340A; US FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection (with limitations). Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: ASTM D 3350 PE224340A; US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Processing Method: Blown Film; Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccASTM D792
ESCR 100% Igepal® >= 2000 hourF0; ASTM D1693C
 >= 1500 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 40 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56Compression molded parts prepared according to ASTM D1928 Procedure C; ASTM D2240
 61Plaque molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 3000 psiCompression molded parts prepared according to ASTM D1928 Procedure C; ASTM D638
 3100 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 2750 psiCompression molded parts prepared according to ASTM D1928 Procedure C; ASTM D638
 2900 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 700 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
 >= 800 %Compression molded parts prepared according to ASTM D1928 Procedure C; ASTM D638
Elongation at Yield 4.0 %Plaque molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 87000 psi2% Secant, Plaque molded and tested in accordance with ASTM D4976; ASTM D790B
 95000 psiMethod I (3 point load) Compression molded parts prepared according to ASTM D1928 Procedure C; ASTM D790B
Tensile Impact Strength 110 ft-lb/in²Plaque molded and tested in accordance with ASTM D4976, Type S; ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Melting Point 259 °F
Crystallization Temperature 239 °FPeak
Deflection Temperature at 0.46 MPa (66 psi) 131 °FUnannealed; ASTM D648
Vicat Softening Point 248 °FASTM D1525
Brittleness Temperature <= -139 °FCompression molded parts prepared according to ASTM D1928 Procedure C; ASTM D746
 <= -105 °FPlaque molded and tested in accordance with ASTM D4976; ASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 440 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF486 / 311179

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.