MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Vistalon™ 7500 Bimodal EPDM Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vistalon 7500 EPDM rubber is a grade of high molecular weight with a low ethylene content and a high diene level. It is produced with ExxonMobil Chemical's proprietary technology offering bimodal molecular weight distribution (MWD). This grade is ideal for the manufacturing of profiles and hoses combining high collapse resistance and smooth extrusion.

Key Features:

  • Consistent quality of mixed compound.
  • Improved productivity of mixing, extrusion and molding.
  • Reduced inventories by using a single grade.
  • High collapse resistance.
  • High elasticity with easy processing.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 82
@Temperature 125 °C
ML 1 + 4; ASTM D1646
 
Descriptive Properties
ENB Content5.7%ASMT D6047
Ethylene Content56%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 4570 EPDM Hydrocarbon Rubber
ExxonMobil Vistalon™ 5601 Metallocene EPDM
Avient Elastamax™ XL 0162-21 EPDM TPV-Based Thermoplastic Elastomer
ExxonMobil Vistalon™ 5600 Metallocene EPDM
ExxonMobil Vistalon™ 7001 Metallocene EPDM

PEXB332 / 37637

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.