MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema Rilsamid® ASR 13 PA12-CF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %Dry; Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Dry; Sim. to ISO 62
Melt Flow >= 10 g/10 min>= 10 g/10 minASTM D1238
 10 g/10 min
@Load 5.00 kg,
Temperature 235 °C
10 g/10 min
@Load 11.0 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiCond.; ISO 527-1/-2
 127 MPa18400 psiDry; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %Cond.; ISO 527-1/-2
Tensile Modulus 9.00 GPa1310 ksiCond.; ISO 527-1/-2
 9.60 GPa1390 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
 4.70 J/cm²
@Temperature -30.0 °C
22.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 4.80 J/cm²
@Temperature -30.0 °C
22.8 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1e+051e+05Cond.; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F10°C/min; Dry; ISO 11357-1/-3
Decomposition Temperature 223 °C433 °F1% wt. loss, TGA, in air
 223 °C433 °F1% wt. loss, TGA, in nitrogen
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 60.0 °C140 °FInjection Molding; ISO 10724
Hold Pressure 19.0 MPa2760 psiInjection Molding; ISO 294
 
Descriptive Properties
ConductiveYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® S223-G2U PA66-GF13, Dry, 13% Glass Filled
Hexcel® HexTow® PV42/850 Carbon Fiber
Toho Tenax Besfight® G30-700 12K HTA-7C EP03 Continuous Filament Carbon Fiber
Envalior Durethan® BCF 30 X H2.0 901510 Nylon 6 (PA6), 30% Glass/Carbon Fiber Reinforced, Dry
Solvay Thornel® Mat VME Carbon Fiber

PARKF862 / 193610

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.