MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technology with a variety of polymers to produce high performance SHINSTRA compound. SHINSTRA compounds are designed by alloying engineering thermoplastics or mineral reinforcing or fiber reinforcing or hybrid filler reinforcing. SHINSTRA are tailored to control the mechanical and physical properties according to its application or customer demand. SHINSTRA are often used to replace metal parts.

    Feature and Benefits
  • Excellent impact resistance
  • High scratch resistance
  • Outstanding abrasion resistance
  • Excellent chemical resistance
  • Excellent mechanical properties
  • Improved thermal properties
  • Easy processing
  • Lighter weight
  • Cost effective

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 854 kg(f)/cm²
Elongation at Break 4.0 %
Flexural Strength 113.8 MPa
Flexural Modulus 52000 kg(f)/cm²
Izod Impact, Notched 4.00 kg-cm/cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shinil Chemical SHINSTRA PC/ABS SCV2030 Structural Polymer Housing
LNP Thermocomp® 9760 Polycarbonate + PBT Alloy, Mineral Filler
Celanese SO.F.TER Reblend® 5510M4 20% Mineral-filled PC/ABS alloy
Avient Edgetek® PC-30GF-20MN/000 Polycarbonate (PC), Glass/Mineral Filled

PSHINL43 / 104045

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.