MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Paper match is a multi layer graphic sheet. The core layer is a high rigidity PP. The skin layers are high field polyolefine. The surface bonds easily to inks and have some absorbing capacity.

Main advantages are: High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy processing with conventional paper converting equipment.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
Thickness 400 microns
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 28.0 MPa
@Temperature 23.0 °C
ASTM D638
Film Tensile Strength at Yield, TD 26.0 MPa
@Temperature 23.0 °C
ASTM D638
Film Elongation at Break, MD >= 100 %
@Temperature 23.0 °C
ASTM D638
Film Elongation at Break, TD >= 100 %
@Temperature 23.0 °C
ASTM D638
Film Elongation at Yield, MD 14 %
@Temperature 23.0 °C
ASTM D638
Film Elongation at Yield, TD 9.4 %
@Temperature 23.0 °C
ASTM D638
Modulus of Elasticity 0.800 GPa
@Temperature 23.0 °C
MD/TD; ASTM D638
Tear Strength <= 230 kN/mMapal internal
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 145 °CASTM D1525
Heat Distortion Temperature 110 °CASTM 648
 
Descriptive Properties
Yield (g/m²)416

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Mapal Plastics Maplon Type D Polypropylene Sheet
Mapal Plastics Maplon Type H Polypropylene Sheet
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet

PMAPAL07 / 83618

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.