Multi-Flex® G 7150 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactured by Shell, under the reference Kraton G 7150 and complies to the internal specifications of Shell/Multibase. The burn rate is 0.7 in/min (217.5 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G. Data provided by Multibase. |