MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® NA960083 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good uniformity, ease of processing and good tensile strength.

Regulatory Status
The basic resin NA 960 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing NA 960 can only be made when the processing conditions, equipment and end use are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Thickness 1.25 mil2:1 BUR; 25 mil die gap
Melt Flow 0.90 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2100 psiData derived from type IV specimen, 75 mil plaque @ 20" min.; ASTM D638
Film Elongation at Break, MD 200 %ASTM D882
Film Elongation at Break, TD 500 %ASTM D882
Elongation at Break 660 %Molded; ASTM D638
Elmendorf Tear Strength MD 300 gASTM D1922
Elmendorf Tear Strength TD 130 gASTM D1922
Dart Drop Test 120 gF50; ASTM D1709
Film Tensile Strength at Break, MD 3500 psiASTM D882
Film Tensile Strength at Break, TD 2400 psiASTM D882
1% Secant Modulus, MD 29000 psiASTM D882
1% Secant Modulus, TD 34000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 92.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 350 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
AntiblockMedium
SlipNone

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA963083 Low Density Polyethylene
LyondellBasell Petrothene® NA963046 Low Density Polyethylene, Film Extrusion Grade
LyondellBasell Petrothene® NA960000 Low Density Polyethylene
LyondellBasell Petrothene® NA940000 Low Density Polyethylene, Blow Molding Data
LyondellBasell Petrothene® NA350136 Low Density Polyethylene

PEQU0501b / 36968

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.