MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huafon JF-P-2922/JF-I-2918 Polyester
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Characteristics: Low hardness and low density.

Applications: For the functional shoes, insoles.

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.140 - 0.180 g/ccFree rise foam density
 0.260 - 0.320 g/ccMolded
 1.14 - 1.18 g/cc
@Temperature 40.0 °C
JF-P-2922
 1.18 - 1.20 g/cc
@Temperature 40.0 °C
JF-P-2918
Viscosity 200 - 500 cP
@Temperature 40.0 °C
JF-P-2918
 1200 - 1600 cP
@Temperature 40.0 °C
JF-P-2922
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1.20 MPa
Elongation at Break >= 350 %
Tear Strength >= 5.00 kN/m
 
Processing PropertiesOriginal ValueComments
Mold Temperature 35.0 - 55.0 °C
 
Descriptive Properties
AppearanceLiquid or waxy40°C, JF-P-2922
 Transparent and pure liquid40°C, JF-I-2918
Asker C Hardness22-30
Cream time7-9 sec
Demold time5-7 min
Material Temperature38-42°C
P+C/l Mix ratio100/68-70
Rise time60-80 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHUAF027 / 294970

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.