MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® FR-10110 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.160 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 216 psiParallel to Rise; ASTM D1623
 218 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 340 psiRise Parallel to Test Span; ASTM D790
 343 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 16114 psiRise Parallel to Test Span; ASTM D790
 16887 psiRise Parallel to Beam Thick.; ASTM D790
Compressive Strength 222 psi
@Temperature 177 °C
Parallel to Rise; ASTM D1621
 273 psi
@Temperature 177 °C
Perpendicular to Rise; ASTM D1621
 339 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 359 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 470 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 483 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
Compressive Modulus 5794 psi
@Temperature 177 °C
Parallel to Rise; ASTM D1621
 6823 psi
@Temperature 177 °C
Perpendicular to Rise; ASTM D1621
 8260 psi
@Temperature 121 °C
Parallel to Rise; ASTM D1621
 8294 psi
@Temperature 121 °C
Perpendicular to Rise; ASTM D1621
 10654 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 10780 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Poissons Ratio 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.0 µin/in-°F
@Temperature -28.9 - 71.1 °C
GP Method
Thermal Conductivity 0.270 BTU-in/hr-ft²-°FASTM C518
 
Descriptive Properties
Tumbling Friability (%)2620 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3830 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3808 FST Polyurethane Foam

PGENR060 / 186846

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.