MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Lewisol™ 29-M Resin
Categories: Other Engineering Material

Material Notes: Product Description: Lewisol™ 29-M resin is a glycero-ester of rosin modified with maleic anhydride. This is a hard, thermoplastic resin with particularly low color that offers excellent solubility, good solvent evaporation, good resistance to oxidation and low viscosity in solution for making RSNitrocellulose lacquers. These and other properties make Lewisol™ 29-M resins particularly suitable for use in lacquers, low temperature heat cured enamels; RS Nitrocellulose based printing inks, and grease resistant coatings.

Application/Uses:

  • Caulks and Sealants
  • Graphic Arts
  • Paint and Coatings

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 1.00 g/cc
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 40[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 123 °CASTM E 28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number >= 4.0
 
Descriptive Properties
Appearancelight amber crystalline solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5346 / 222540

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.