MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron™ D7015G PI Bearing Grade Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: This hot compression molded, 15% graphite filled PI is a bearing grade material with superior temperature and wear resistance, as well as a low coefficient of friction.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Water Absorption at Saturation 3.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 115ASTM D785
Hardness, Shore D 86.0ISO 868
Tensile Strength 105 MPaISO 527-1/-2 (7)
Flexural Strength 150 MPaISO 178 (12)
Compressive Yield Strength 40.0 MPa
@Strain 1.00 %
ISO 604 (10)
 70.0 MPa
@Strain 2.00 %
ISO 604 (10)
 130 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 90.0 MPaASTM D732
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 10000 ohmANSI/ESD STM 11.11
Dielectric Strength 13.0 kV/mmIEC 60243-1 (15)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°FASTM E-831 (TMA)
 37.0 µm/m-°C
@Temperature 23.0 - 100 °C
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
 49.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.390 W/m-K
 2.70 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 570 °FContinuous Use Temperature in Air after 20000 hr
Minimum Service Temperature, Air -321 °F
 -196 °C
Glass Transition Temp, Tg 735 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Unacceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ESd categoryConductive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
DuPont Mobility and Materials Vespel® SP-21 Polyimide, 15% Graphite Filled, Direct formed
Mitsubishi Chemical Advanced Materials Duratron™ CU60 PBI Polybenzimidazole, unfilled, compression molded
KEP Kepital® F10-03H Acetal Copolymer, High viscosity, High rigidity

P1SM05u / 104385

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.