MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® K102 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape; Thermoset; Polyimide, TS

Material Notes: CHR® K102 is manufactured from polyimide film with high-temperature adhesive.

Features/Benefits: CHR® K102 has excellent mechanical and electrical properties, plus excellent dielectric strength. CHR® K102 offers high temperature resistance and a high conformability/resistance to solvents. CHR® K102 has an outstanding resistance to cut through, and is impact and abrasion resistant. Acrylic adhesive can be thermoset. The polyimide backing meets MIL-P-46112B.

Applications: CHR® K102 is constructed to fill the requirements of high performance thermoplastic polyimide backing materials. CHR® K102 was designed to fill the need of non-silicone adhesive gold finger connector wave solder protection. CHR® K102 works well for both solvent and water based fluxes. CHR® K102 fills the various needs in electronic assembly and electrical insulation applications.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 50 %
Tear Strength 30.0 pliInitial Tear Strength
Peel Strength 0.330 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 7000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -20.0 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 383 Acrylic Adhesive
Saint-Gobain CHR® K103 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2819-3(R) Acrylic Adhesive Zone Tape
Permabond TA430 Acrylic Adhesive & Initiator
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive

PSTGQZ334 / 68848

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.