MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polycarbonate, Carbon + PTFE Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon + PTFE Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.27 - 1.55 g/ccAverage value: 1.36 g/cc Grade Count:63
Filler Content 10.0 - 40.0 %Average value: 19.8 % Grade Count:28
Water Absorption 0.0600 - 0.310 %Average value: 0.118 % Grade Count:32
Additive Loading 10.0 - 20.0 %Average value: 13.8 % Grade Count:4
Linear Mold Shrinkage 0.000 - 0.0100 cm/cmAverage value: 0.00172 cm/cm Grade Count:56
Linear Mold Shrinkage, Transverse 0.000800 - 0.00500 cm/cmAverage value: 0.00373 cm/cm Grade Count:9
Melt Flow 5.50 - 20.0 g/10 minAverage value: 10.8 g/10 min Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116 - 120Average value: 118 Grade Count:5
Tensile Strength, Ultimate 89.6 - 193 MPaAverage value: 120 MPa Grade Count:64
Tensile Strength, Yield 91.7 - 129 MPaAverage value: 110 MPa Grade Count:7
Elongation at Break 1.00 - 10.0 %Average value: 2.60 % Grade Count:60
Elongation at Yield 1.90 - 6.00 %Average value: 2.97 % Grade Count:10
Modulus of Elasticity 6.89 - 24.1 GPaAverage value: 12.1 GPa Grade Count:46
Flexural Yield Strength 109 - 255 MPaAverage value: 179 MPa Grade Count:61
Flexural Modulus 6.21 - 21.7 GPaAverage value: 10.9 GPa Grade Count:59
Izod Impact, Notched 0.427 - 3.50 J/cmAverage value: 0.992 J/cm Grade Count:59
Izod Impact, Unnotched 0.801 - 8.54 J/cmAverage value: 5.11 J/cm Grade Count:44
Izod Impact, Notched (ISO) 7.20 - 8.95 kJ/m²Average value: 8.05 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) 22.0 - 34.0 kJ/m²Average value: 27.8 kJ/m² Grade Count:5
Charpy Impact Unnotched 3.00 - 4.50 J/cm²Average value: 3.58 J/cm² Grade Count:6
 2.50 - 4.00 J/cm²
@Temperature -40.0 - -30.0 °C
Average value: 3.50 J/cm² Grade Count:3
Charpy Impact, Notched 0.800 - 1.20 J/cm²Average value: 0.960 J/cm² Grade Count:5
 0.900 - 0.900 J/cm²
@Temperature -40.0 - -30.0 °C
Average value: 0.900 J/cm² Grade Count:3
Falling Dart Impact 11.3 - 16.1 JAverage value: 13.5 J Grade Count:8
Instrumented Impact Total Energy 2.62 - 4.02 JAverage value: 3.14 J Grade Count:4
Coefficient of Friction 0.160 - 0.430Average value: 0.292 Grade Count:5
Coefficient of Friction, Static 0.130 - 0.340Average value: 0.222 Grade Count:5
K (wear) Factor 7.00 - 76.5 x 10-8 mm³/N-MAverage value: 30.8 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00 - 1.00e+7 ohm-cmAverage value: 151000 ohm-cm Grade Count:42
Surface Resistance 10.0 - 1.00e+6 ohmAverage value: 240000 ohm Grade Count:24
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 - 40.0 µm/m-°CAverage value: 29.4 µm/m-°C Grade Count:10
CTE, linear, Transverse to Flow 32.0 - 45.0 µm/m-°CAverage value: 38.0 µm/m-°C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 135 - 151 °CAverage value: 145 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 123 - 149 °CAverage value: 142 °C Grade Count:54
Vicat Softening Point 147 - 160 °CAverage value: 151 °C Grade Count:6
Flammability, UL94 HB - V-0Grade Count:44
 
Processing PropertiesOriginal ValueComments
Processing Temperature 249 - 293 °CAverage value: 271 °C Grade Count:15
Nozzle Temperature 271 - 316 °CAverage value: 293 °C Grade Count:12
Melt Temperature 254 - 330 °CAverage value: 295 °C Grade Count:42
Mold Temperature 48.9 - 130 °CAverage value: 92.3 °C Grade Count:57
Drying Temperature 100 - 130 °CAverage value: 120 °C Grade Count:42
Moisture Content 0.0200 %Average value: 0.0200 % Grade Count:33
Dew Point -28.9 °CAverage value: -28.9 °C Grade Count:17
Injection Pressure 68.9 - 103 MPaAverage value: 86.2 MPa Grade Count:32
Vent Depth 0.00250 - 0.00760 cmAverage value: 0.00505 cm Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
Overview of materials for Polycarbonate, Glass + PTFE Filled
Overview of materials for Polycarbonate, 30% Glass Filled
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
Overview of materials for Polycarbonate, 20% Glass Filled

O3127 / 78139

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.