MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MarkeTech Resorcinol Formaldehyde Aerogel  (discontinued **)
Categories: Ceramic; Aerogel

Material Notes: Monolithic resorcinol formaldehyde (RF) nanofoams are primarily used as the precursor for carbon nanofoams or when an organic, electrically insulating material is desired. The standard RF nanofoam is offered as a high density material of 0.6 g/cm. Researchers wanting to control the pyrolysis conditions (atmosphere, temperature, time, etc.) during the processing of a carbon nanofoam can begin with RF nanofoam. Monolithic RF nanofoams are available as random pieces 0.2 to 2.0 cm in size. RF nanofoam sheets are formed by impregnating non-woven carbon paper with the RF gel. After processing, the resultant sheet is nominally 0.012" thick and has a density of 0.6 g/cm3. The overall sheet size is 3.5 x 10 cm.

Data provided by the supplier, MarkeTech International.

MarkeTech International is no longer in business.

Key Words: Aerogels
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.600 g/cc
Specific Surface Area 600 m²/g
Thickness 12.0 mil
 
Mechanical PropertiesOriginal ValueComments
Compressive Modulus 0.300 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 2.0
@Frequency 1.80e+10 - 4.00e+10 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 - 80.0 °C
Thermal Conductivity 0.0600 W/m-K
 
Descriptive Properties
ColorDark Red

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
MarkeTech Carbon Aerogel
MarkeTech Carbon Nanofoam
Aluminum 356.0-T7, Sand Cast
Aluminum B356.2 Composition Spec

C5MTO2 / 373

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.