MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EN 1.0045 High Manganese Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Key Words: EN 10025(90)A1(93) 1.0045. Similar to ASTM A678(C), UNS K02204
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccEstimated by MatWeb from similar grade
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 450 - 630 MPa
@Thickness 200 - 250 mm
Structural, Hot Rolled, Base Steel
 490 - 630 MPa
@Thickness 63.0 - 80.0 mm
Structural, Hot Rolled, Base Steel
 490 - 630 MPa
@Thickness 3.00 - 16.0 mm
Structural, Hot Rolled, Base Steel
 510 - 680 MPa
@Thickness <=1.00 mm
Structural, Hot Rolled, Quality Steel
 510 - 680 MPa
@Thickness <=1.00 mm
Structural, Hot Rolled, Base Steel
Tensile Strength, Yield 275 MPa
@Thickness 200 - 250 mm
Structural, Hot Rolled, Base Steel
 325 MPa
@Thickness 63.0 - 80.0 mm
Structural, Hot Rolled, Base Steel
 355 MPa
@Thickness <=1.00 mm
Structural, Hot Rolled, Quality Steel
 355 MPa
@Thickness 3.00 - 16.0 mm
Structural, Hot Rolled, Base Steel
 355 MPa
@Thickness <=1.00 mm
Structural, Hot Rolled, Base Steel
Elongation at Break 12 %
@Thickness <=1.00 mm
Transverse. Structural, Hot Rolled, Quality Steel
 12 %
@Thickness <=1.00 mm
Transverse. Structural, Hot Rolled, Base Steel
 14 %
@Thickness <=1.00 mm
Longitudinal. Structural, Hot Rolled, Quality Steel
 14 %
@Thickness <=1.00 mm
Longitudinal. Structural, Hot Rolled, Base Steel
 17 %
@Thickness 200 - 250 mm
Longitudinal. Structural, Hot Rolled, Base Steel
 17 %
@Thickness 200 - 250 mm
Transverse. Structural, Hot Rolled, Base Steel
 18 %
@Thickness 63.0 - 80.0 mm
Transverse. Structural, Hot Rolled, Base Steel
 20 %
@Thickness 63.0 - 80.0 mm
Longitudinal. Structural, Hot Rolled, Base Steel
 20 %
@Thickness 3.00 - 16.0 mm
Transverse. Structural, Hot Rolled, Base Steel
 22 %
@Thickness 3.00 - 16.0 mm
Longitudinal. Structural, Hot Rolled, Base Steel
Modulus of Elasticity 200 GPaEstimated by MatWeb from similar grade
Poissons Ratio 0.29Estimated by MatWeb from similar grade
Shear Modulus 80.0 GPaEstimated by MatWeb from similar grade
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cmEstimated by MatWeb from similar grade
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CEstimated by MatWeb from similar grade
Specific Heat Capacity 0.470 J/g-°CEstimated by MatWeb from similar grade
Thermal Conductivity 52.0 W/m-KEstimated by MatWeb from similar grade
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.24 %
Iron, Fe >= 97.5 %
Manganese, Mn <= 1.6 %
Nitrogen, N <= 0.0090 %N max n/a if Al >= 0.020
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.55 %
Sulfur, S <= 0.045 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EN 1.0044 High Manganese Carbon Steel
EN S355K2G3 High Manganese, Structural, Hot Rolled, Quality Steel
EN SA355J2G3 High Manganese, Structural, Hot Rolled, Quality Steel
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
EN 1.0577 High Manganese, Structural, Hot Rolled, Quality Steel

M9ZE10045 / 233227

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.