MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C18625, TD04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Solution Heat Treated and Cold Worked: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed

Typical Uses: Automotive electrical terminals; Connectors, automotive; Heater Cores; Relays; Sensor Bodies; Connectors for High Temperatures; Electrical Conductors; Wire, Electrical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 70
Tensile Strength >= 54.0 ksi
 61.0 ksiTypical
Tensile Strength, Yield >= 51.0 ksi0.2% Offset
 58.0 ksi0.2% Offset, Typical
Elongation at Break >= 20 %
Tensile Modulus 17400 ksi
Modulus of Rigidity 6500 ksi
Poissons Ratio 0.33
Machinability 20 %
Forgeability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm85% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 100 °C
Thermal Conductivity 195 BTU-in/hr-ft²-°F
Melting Point 1967 - 1976 °F
Solidus 1967 °F
Liquidus 1976 °F
Annealing Point >= 1110 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 570 °FStress Relief
Precipitation Temperature >= 930 °F
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 0.15 - 0.35 %
Copper, Cu >= 99.4 %
Nickel, Ni <= 0.10 %
Phosphorus, P 0.050 - 0.090 %
Tin, Sn 0.010 - 0.10 %
Zinc, Zn <= 0.10 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC18625x1 / 291660

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.