MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BiologiQ BioBlend® XD 22620 Biopolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description:
  • A member of the BioBlend® XD Family of Durable BioPolymers for blow molding.
  • BioBlend® XD 22620 contains 20% NuPlastiQ compounded with HDPE.
  • Made from 20% annually renewable agricultural resources.
  • BioBlend® XD 22620 is supplied in pellet form.
  • This TDS covers the following BioBlend® XD BioPolymers: XD 22620 and XD 22621
Applications:
  • BioBlend® XD 22620 is designed for blow molding applications that require stress crack resistance, rigidity, and high impact strength.

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 1.08 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16.2 MPaASTM D638
Flexural Modulus 618 MPaASTM D790
1% Secant Modulus 650 MPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Drying Temperature 60.0 °C
@Time 3600 - 14400 sec
warm, dry air
Moisture Content <= 0.50 %ASTM D6980

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBIOLQ511 / 250871

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.