MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy
Categories: Metal; Ferrous Metal; Superalloy; Iron Base

Material Notes: All values may vary dependent on specific design and usage

99.9% copper cladding over iron-nickel core

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM F29
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.299 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80000 psiAnnealed
 100000 psiStress relieved
 125000 psiHard
Tensile Strength, Yield 50000 psiAnnealed
 70000 psiStress relieved
 100000 psiHard
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 58.0 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 10.28 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 57 - 59 %Core, as balance
Nickel, Ni 41 - 43 %Core

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
California Fine Wire Alloy 52 Nickel Iron Alloy
Kennametal Stellite Nucalloy® 41 Nickel-Chromium-Boron Alloy
Nickel Iron Alloy 52 Sealing Wire, UNS N14052
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600

NCALZ01 / 15544

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.