MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds Mold Max® 60 High Heat Resistant Silicone Rubber Compound
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Mold Max™ 60 is a Shore 60A tin catalyzed silicone rubber formulated for applications requiring high heat resistance (up to 560°F/294°C). It features a low mixed viscosity and cured rubber exhibits very low linear shrinkage. Parts A & B are mixed 100A & 3B by weight. Pot life is 40 minutes and cure time is 24 hours. Applications include making foundry patterns, flat pattern reproductions and casting low-melt metal alloys such as tin and pewter. PLEASE NOTE: THI-VEX™ Silicone Thickener is NOT recommended for use with Mold Max™ 60. Important; you must weigh Part A & B components using a gram scale to be successful with Mold Max™ 60

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D-1475
Viscosity 20000 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0015 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D-2240
Tensile Strength 398 psiASTM D-412
Elongation at Break 135 %ASTM D-412
100% Modulus 331 psiASTM D-412
Tear Strength 63.0 pliDie B; ASTM D-624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+14 ohm-cm
Dielectric Constant 3.4
@Frequency 100 Hz
Dielectric Strength >= 500 V/mil
Dissipation Factor 0.020
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.347 W/m-K
Maximum Service Temperature, Air 294 °C
Minimum Service Temperature, Air -53.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
Pot Life 40.0 minASTM D-2471
 
Descriptive Properties
ColorRed
Mix Ratio100A:3Bby weight
Specific Volume19.1[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN107 / 296808

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.