MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Chockfast® MS-440G Epoxy Nonskid Deck Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: MS-440G is a high solid, two-part, general purpose nonskid deck coating designed to provide maximum wear and impact resistance for US Naval vessels. Fire retardant in the cured state, MS-440G is formulated with epoxy resins to give maximum adhesion to steel, toughness and corrosion resistance. It is resistant to fire and jet blast, most acids, alkali’s, solvents, grease, oil, salt water, detergents, alcohol, gasoline, jet fuels, cellulube and other hydraulic fluids. Because of its tenacious bond, rust will not creep under the coating if fractured. In accordance with NAVSEA guidance to non-skid systems, MS-440G is designed to be used in conjunction with the following American Safety Technologies MIL-SPEC and NAVSEA approved products: MS-7CZ Primer and MS-200/ MS-201 Color Topping.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 90 %+/- 2%
Volatile Organic Compounds (VOC) Content 215 g/l
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 102 °Fmixed
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthMIL-PRF 24667. Requirement

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9039 / 239549

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.